Illustrative imageTPU family
TPU (softer grades)
Softer than 95A, down to gel-like grades such as 85A.
TPU is sold in different Shore hardness grades. Lower numbers, such as 90A or 85A, are softer and stretch more. They are also harder to feed and print, and usually need a direct-drive extruder and very slow speeds.
Properties
General comparison between materials, from 1 to 5. Not lab measurements.
Print settings
- Nozzle temperature
- 220–250 °C
- Bed temperature
- 30–50 °C
- Print speed
- Very slow speeds
- Finish
- Satin, soft touch
- Drying
- Must be dried before printing and kept dry while printing.
- Enclosure & ventilation
- Not required. Prints best with good airflow.
- Storage
- Airtight dry box with fresh desiccant. Absorbs moisture from the air quickly.
- Printer compatibility
- AMS compatibility
Temperatures are general ranges and change with brand and formula. The manufacturer’s data sheet always comes first.
Recommended for
- Soft grips and pads
- Wearable pieces
- Vibration dampers
Not recommended for
- Rigid structural parts
- Sharp, thin decorative detail
- Parts that need tight dimensional accuracy